- Pipe Fittings[1]
- Valves[1]
- Cast & Forged[2]
- Other Metals & Metal Products[10]
- Other Steel Products[10]
- Stainless Steel Pipes[1]
- Steel Pipes[5]
- Steel Sheets[4]
- Steel Strips[2]
- Contact Person : Mr. FSA FSA
- Company Name : Shanghai Fengqu Super Alloy Co., Ltd.
- Tel : 86-21-69155989
- Fax : 86-21-69151848
- Address : Shanghai,Shanghai,NO.101, Boxue road, Malu town, Jiading district
- Country/Region : China
- Zip : 201801
Related Product Searches:Invar pipe,High Quality,Invar pipe, invar pipe
Characteristic:36 alloy is a special ultra-low coefficient of heat expansion of low-iron-nickel alloy. One of carbon and manganese element of control is very important. Cold deformation can reduce the coefficient of thermal expansion, in particular within the framework of the heat treatment temperature coefficient of thermal expansion will enable stabilization. Has the following characteristics:1.Has very low coefficient of heat expansion between the temperature of -250 and 200.2.Good toughness and plastic
Metallurgical structureInvar 36 is the face centered cubic lattice structure
Corrosion resistanceInvar 36 has corrosion resistance in the dry air of room temperature.In other harsh environments, such as the humid air, there may be corrosion (rust).
Applied fieldInvar 36 suit for need to apply ultra-low coefficient of heat expansion environment.Typical applications are as follows:1.Liquefied gas production, storage and transport 2.The measurement and control instruments work temperature lower than 200, such as temperature regulating device 3.Metals and other materials use the screw connector bush 4.Bimetal and bimetallic temperature controller5.Film framework6.Shadow mask 7.CRP components of the aviation industry temper Die 8.lower than -200 the satellite and missile electronic control unit framework 9.The auxiliary tube of the electromagnetic lens in the laser control device
Invar pipe